 Spot welding with Super-MIG®:
Joint type: Spot welding
Material Spec.: High Strength Boron Steel
Position: Flat
Material Thickness: 1.8mm + 1.8mm
Filler Wire: ER70S-6, .035”
Welding Time: 0.5s |
| .jpg) Wire Feed Speed: 16m/min (630ipm)
Plasma Arc: 160A
Plasma Gas: Argon
MIG Voltage: 25V
Shielding Gas: 75%Argon + 25%CO2 |
|
|
|
|